Grades | Stainless Steels | A 1018 HSLAS Grade 65 [450] Class 1 B

SAE A 1018 HSLAS Grade 65 [450] Class 1 B ( Martensite )

PDF | Word | Print

A 1018 HSLAS Grade 65 [450] Class 1 B Application:Steel, Sheet and Strip, Heavy-Thickness Coils, Hot-Rolled, Carbon, Commercial, Drawing, Structural, High-Strength Low-Alloy, High-Strength Low-Alloy with Improved Formability, and Ultra-High Strength Steel

Chemical composition(mass fraction)(wt.%) of the A 1018 HSLAS Grade 65 [450] Class 1 B
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 0.30 0.60
Si 0.50 1.00
P - 0.03
S - 0.03
Cr 8.00 10.00
Ni - -
Mo 0.90 1.10

Mechanical properties of grade A 1018 HSLAS Grade 65 [450] Class 1 B

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
355 (≥) 462 (≥) 23 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade A 1018 HSLAS Grade 65 [450] Class 1 B

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
551 (≥) 582 (≥) 41 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
443 464 562 - - -

A 1018 HSLAS Grade 65 [450] Class 1 B Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED